[an error occurred while processing this directive]The Research on Hydrothermal Aging of Rubber Components for SRM
Received date: 2011-11-01
Online published: 2025-05-29
常新龙 , 刘万雷 , 程建良 , 姜帆 , 赖建伟 . 固体火箭发动机密封件湿热老化性能研究[J]. 弹箭与制导学报, 2012 , 32(4) : 222 -224 . DOI: 10.15892/j.cnki.djzdxb.2012.04.014
A hydrothermal accelerated aging test based on F108 fluorine rubber of SRM was investigated to explore aging mechanism and performance deterioration law. The experimental results were analyzed with mathematical statistics. The results show the temperature is the most significant factor for fluorine rubber's ageing, and the humidity accelerates aging speed.
| [1] | 胡殿印, 王荣桥, 任全彬,等. 固体火箭发动机O形圈密封技术综述[J]. 北京航空航天大学学报, 2005, 31 (2): 95- 100. |
| [2] | 中国石油和石化工程研究会. 当代石油和石化工业技术普及读本[M]. 北京: 中国石化出版社, 2000. |
| [3] | Cynthia L Lach. Effect of temperature and gap opening rate on the resiliency of canditate solid rocket booster o-ring materials[R]. NASA Technical Paper, 1996, 3226. |
| [4] | 孙兵晓, 常新龙, 胡成荣,等. 固体火箭发动机密封结构随机有限元可靠性分析[J]. 火箭推进, 2008, 34 (5): 22- 23. |
| [5] | 陈经盛. 橡胶湿热老化试验的研究[J]. 老化与应用, 1994 (1): 1- 7. |
| [6] | 卢黎明. 浅析橡胶密封圈的压缩率对密封性能的影响[J]. 润滑与密封, 2003 (4): 85- 86. |
/
| 〈 |
|
〉 |