CORRELATION TECHNOLOGY

The Research on Hydrothermal Aging of Rubber Components for SRM

  • CHANG Xinlong ,
  • LIU Wanlei ,
  • CHENG Jianliang ,
  • JIANG Fan ,
  • LAI Jianwei
Expand
  • 1 The Second Artillery Engineering University, Xi'an 710025, China
    2 The Second Artillery Equipment Academy, Beijing 100085, China

Received date: 2011-11-01

  Online published: 2025-05-29

Abstract

A hydrothermal accelerated aging test based on F108 fluorine rubber of SRM was investigated to explore aging mechanism and performance deterioration law. The experimental results were analyzed with mathematical statistics. The results show the temperature is the most significant factor for fluorine rubber's ageing, and the humidity accelerates aging speed.

Cite this article

CHANG Xinlong , LIU Wanlei , CHENG Jianliang , JIANG Fan , LAI Jianwei . The Research on Hydrothermal Aging of Rubber Components for SRM[J]. Journal of Projectiles, Rockets, Missiles and Guidance, 2012 , 32(4) : 222 -224 . DOI: 10.15892/j.cnki.djzdxb.2012.04.014

References

[1]
胡殿印, 王荣桥, 任全彬,等. 固体火箭发动机O形圈密封技术综述[J]. 北京航空航天大学学报, 2005, 31 (2): 95- 100.
[2]
中国石油和石化工程研究会. 当代石油和石化工业技术普及读本[M]. 北京: 中国石化出版社, 2000.
[3]
Cynthia L Lach. Effect of temperature and gap opening rate on the resiliency of canditate solid rocket booster o-ring materials[R]. NASA Technical Paper, 1996, 3226.
[4]
孙兵晓, 常新龙, 胡成荣,等. 固体火箭发动机密封结构随机有限元可靠性分析[J]. 火箭推进, 2008, 34 (5): 22- 23.
[5]
陈经盛. 橡胶湿热老化试验的研究[J]. 老化与应用, 1994 (1): 1- 7.
[6]
卢黎明. 浅析橡胶密封圈的压缩率对密封性能的影响[J]. 润滑与密封, 2003 (4): 85- 86.